屈服强度提高12.6%
该修复层在30米水深下通过激光熔覆直接沉积成形,与X70基体形成冶金结合,其细晶与高位错组织显著提升强度。
Wang, Zhandong · Chunke, Wang · Linzhong, Wu · Jia, Zhiyuan · Chen, Mingzhi · Lan, Huifang · 孙桂芳
Materials Science & Engineering A: Structural Materials: Properties, Microstructure and Processing 2026
30米水深修复
位错密度(4.5 ± 0.4) × 10¹⁴ m⁻²